Note
Go to the end to download the full example code.
Oguntoye-60C¶
Data for Main / Vo2 / Oguntoye-60c
import os
import matplotlib.pyplot as plt
import numpy as np
import refidx as ri
plt.style.use("../../doc/refidx.mplstyle")
db = ri.DataBase()
matid = ['main', 'VO2', 'Oguntoye-60C']
mat = db.get_item(matid)
wr = mat.wavelength_range
lamb = np.linspace(*wr, 1000)
index = mat.get_index(lamb)
fig, ax = plt.subplots(2, 1, figsize=(3, 3))
ax[0].plot(lamb, index.real, "-", color="#aa0044")
ax[1].plot(lamb, index.imag, "-", color="#6886b3")
ax[0].set_xlabel(r"Wavelength ($\rm μm$)")
ax[1].set_xlabel(r"Wavelength ($\rm μm$)")
ax[0].set_ylabel(r"$n^{\prime}$")
ax[1].set_ylabel(r"$n^{\prime\prime}$")
plt.suptitle(mat)
mat.print_info(
html=True,
tmp_dir=os.path.join("..","..", "doc", "auto_gallery","VO2"),
filename="out_main_VO2_Oguntoye_60C.html",
)
Comments
~209 nm-thick VO2 film on SiO2 substrate. 60 °C.
References
I. O. Oguntoye, S. Padmanabha, M. Hinkle, T. Koutsougeras, A. J. Ollanik, M. D. Escarra. Continuously tunable optical modulation using vanadium dioxide Huygens metasurfaces, ACS Appl. Mater. Interfaces 15, 41141–41150 (2023) (Numerical data kindly provided by Isaac Oguntoye)
Total running time of the script: (0 minutes 0.387 seconds)
Estimated memory usage: 225 MB