Oguntoye-30C

Data for Main / Vo2 / Oguntoye-30c

import os
import matplotlib.pyplot as plt
import numpy as np
import refidx as ri

plt.style.use("../../doc/refidx.mplstyle")
db = ri.DataBase()
matid = ['main', 'VO2', 'Oguntoye-30C']
mat = db.get_item(matid)
wr = mat.wavelength_range
lamb = np.linspace(*wr, 1000)
index = mat.get_index(lamb)
fig, ax = plt.subplots(2, 1, figsize=(3, 3))
ax[0].plot(lamb, index.real, "-", color="#aa0044")
ax[1].plot(lamb, index.imag, "-", color="#6886b3")
ax[0].set_xlabel(r"Wavelength ($\rm μm$)")
ax[1].set_xlabel(r"Wavelength ($\rm μm$)")
ax[0].set_ylabel(r"$n^{\prime}$")
ax[1].set_ylabel(r"$n^{\prime\prime}$")
plt.suptitle(mat)
mat.print_info(
    html=True,
    tmp_dir=os.path.join("..","..", "doc", "auto_gallery","VO2"),
    filename="out_main_VO2_Oguntoye_30C.html",
)
Material main VO2 Oguntoye-30C
Comments

~209 nm-thick VO2 film on SiO2 substrate. 30 °C.

References

I. O. Oguntoye, S. Padmanabha, M. Hinkle, T. Koutsougeras, A. J. Ollanik, M. D. Escarra. Continuously tunable optical modulation using vanadium dioxide Huygens metasurfaces, ACS Appl. Mater. Interfaces 15, 41141–41150 (2023) (Numerical data kindly provided by Isaac Oguntoye)

Total running time of the script: (0 minutes 0.414 seconds)

Estimated memory usage: 225 MB