Beaini-25C

Data for Main / Vo2 / Beaini-25c

import os
import matplotlib.pyplot as plt
import numpy as np
import refidx as ri

plt.style.use("../../doc/refidx.mplstyle")
db = ri.DataBase()
matid = ['main', 'VO2', 'Beaini-25C']
mat = db.get_item(matid)
wr = mat.wavelength_range
lamb = np.linspace(*wr, 1000)
index = mat.get_index(lamb)
fig, ax = plt.subplots(2, 1, figsize=(3, 3))
ax[0].plot(lamb, index.real, "-", color="#aa0044")
ax[1].plot(lamb, index.imag, "-", color="#6886b3")
ax[0].set_xlabel(r"Wavelength ($\rm μm$)")
ax[1].set_xlabel(r"Wavelength ($\rm μm$)")
ax[0].set_ylabel(r"$n^{\prime}$")
ax[1].set_ylabel(r"$n^{\prime\prime}$")
plt.suptitle(mat)
mat.print_info(
    html=True,
    tmp_dir=os.path.join("..","..", "doc", "auto_gallery","VO2"),
    filename="out_main_VO2_Beaini_25C.html",
)
Material main VO2 Beaini-25C
Comments

70 nm-thick VO2 film deposited on SiO2 substrate. 25 °C.

References

R. Beaini, B. Baloukas, S. Loquai, J.E. Klemberg-Sapieha, L. Martinu. Thermochromic VO2-based smart radiator devices with ultralow refractive index cavities for increased performance, Sol. Energy Mater. Sol. Cells 205, 110260 (2020) (Data points extracted from Fig. 1)

Total running time of the script: (0 minutes 0.366 seconds)