Note
Go to the end to download the full example code.
Ciesielski¶
Data for Main / Se / Ciesielski
import os
import matplotlib.pyplot as plt
import numpy as np
import refidx as ri
plt.style.use("../../doc/refidx.mplstyle")
db = ri.DataBase()
matid = ['main', 'Se', 'Ciesielski']
mat = db.get_item(matid)
wr = mat.wavelength_range
lamb = np.linspace(*wr, 1000)
index = mat.get_index(lamb)
fig, ax = plt.subplots(2, 1, figsize=(3, 3))
ax[0].plot(lamb, index.real, "-", color="#aa0044")
ax[1].plot(lamb, index.imag, "-", color="#6886b3")
ax[0].set_xlabel(r"Wavelength ($\rm μm$)")
ax[1].set_xlabel(r"Wavelength ($\rm μm$)")
ax[0].set_ylabel(r"$n^{\prime}$")
ax[1].set_ylabel(r"$n^{\prime\prime}$")
plt.suptitle(mat)
mat.print_info(
html=True,
tmp_dir=os.path.join("..","..", "doc", "auto_gallery","Se"),
filename="out_main_Se_Ciesielski.html",
)
Comments
25 nm-thick selenium film deposited directly on SiO2 substrate
References
A. Ciesielski, L. Skowronski, W.Pacuski, T. Szoplik. Permittivity of Ge, Te and Se thin films in the 200–1500 nm spectral range. Predicting the segregation effects in silver, Mat. Sci. Semicond. Process. 81, 64-67 (2018) (Numerical data kindly provided by Arkadiusz Ciesielski)
Total running time of the script: (0 minutes 0.383 seconds)
Estimated memory usage: 225 MB