Boidin

Data for Main / Al2o3 / Boidin

import os
import matplotlib.pyplot as plt
import numpy as np
import refidx as ri

plt.style.use("../../doc/refidx.mplstyle")
db = ri.DataBase()
matid = ['main', 'Al2O3', 'Boidin']
mat = db.get_item(matid)
wr = mat.wavelength_range
lamb = np.linspace(*wr, 1000)
index = mat.get_index(lamb)
fig, ax = plt.subplots(2, 1, figsize=(3, 3))
ax[0].plot(lamb, index.real, "-", color="#aa0044")
ax[1].plot(lamb, index.imag, "-", color="#6886b3")
ax[0].set_xlabel(r"Wavelength ($\rm μm$)")
ax[1].set_xlabel(r"Wavelength ($\rm μm$)")
ax[0].set_ylabel(r"$n^{\prime}$")
ax[1].set_ylabel(r"$n^{\prime\prime}$")
plt.suptitle(mat)
mat.print_info(
    html=True,
    tmp_dir=os.path.join("..","..", "doc", "auto_gallery","Al2O3"),
    filename="out_main_Al2O3_Boidin.html",
)
Material main Al2O3 Boidin
Comments

Thin films of amorphous alumina were fabricated using pulsed laser deposition in vacuum.
Influence of deposition parameters, specifically deposition time under vacuum and partial pressure of argon, is discussed in the original publication.

References

R. Boidin, T. Halenkovič, V. Nazabal, L. Beneš, P. Němec. Pulsed laser deposited alumina thin films, Ceramics International 42, 1177-1182 (2016) (Numerical data kindly provided by Tomáš Halenkovič)

Total running time of the script: (0 minutes 0.293 seconds)

Estimated memory usage: 225 MB

Gallery generated by Sphinx-Gallery